{"id":3822,"date":"2020-08-06T02:22:33","date_gmt":"2020-08-06T08:22:33","guid":{"rendered":"https:\/\/www.cast-parts.com\/castings\/porosity-in-die-cast-parts-process-2020\/"},"modified":"2020-08-06T02:22:33","modified_gmt":"2020-08-06T08:22:33","slug":"porosity-in-die-cast-parts-process-2020","status":"publish","type":"post","link":"https:\/\/www.cast-parts.com\/castings\/porosity-in-die-cast-parts-process-2020\/","title":{"rendered":"Porosity in Die Cast Parts Process 2020"},"content":{"rendered":"<p>Porosity in Die Cast Parts Process 2020 &#8211; <\/p>\n<p>The steel die cavity is sprayed with a liquid release agent to prevent the molten metal from sticking to the steel cavity. Much like the cook will spray a pan before baking a cake. The spray dissipates into steam because the die is very hot. Porosity is natural in the Die Casting Process. The molten metal is squirted at a very fast speed and under extreme pressure into the die. It is like a running water hose with a thumb on the nozzle. The metal is moving very rapidly as it is forcibly injected into a steel die cavity, the metal picks up voids and air bubbles from the steam and the turbulence of the injection. The metal is squeezed into the die with a piston to evacuate or to remove and compress most of the voids and air pockets. Those voids and air pockets are called die casting porosity. It is a natural occurrence in the production of die casting parts. To read more about <a href=\"https:\/\/www.kineticdiecasting.com\/porosity.html\" target=\"_blank\" rel=\"noopener noreferrer\">die casting porosity<\/a>, review our web page: <a href=\"https:\/\/www.kineticdiecasting.com\/porosity.html\" target=\"_blank\" rel=\"noopener noreferrer\">https:\/\/www.kineticdiecasting.com\/porosity.html<\/a><\/p>\n<p>Kinetic Die Casting Company 6918 Beck Avenue, North Hollywood, California 91605 USA<br \/>\nE-mail <a href=\"mailto:sales@kineticdc.com\">sales@kineticdc.com<\/a> Toll Free: (800) 524-8083 Local: (818) 982-9200 Fax: (818) 982-0877<\/p>\n<p>Permalink: <a href=\"https:\/\/www.kineticdiecasting.com\/kdc\/porosity-in-the-die-casting-process-2\/\" target=\"_blank\" rel=\"noopener noreferrer\">https:\/\/www.kineticdiecasting.com\/kdc\/porosity-in-the-die-casting-process-2\/<\/a><\/p>\n<p><strong><br \/>\nKinetic Die Casting Company<\/strong><br \/>\nE-mail <a href=\"mailto:sales@kineticdc.com\">sales@kineticdc.com<\/a> \/ 818-982-9200 \/ 800-524-8083 Toll Free \/ 818-982-0877 Fax<br \/>\n6918 Beck Avenue, North Hollywood, California USA 91605,<br \/>\nKineticdc makes:<br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/heatsink.html\" target=\"_blank\" rel=\"noopener noreferrer\">Aluminum Heat Sinks<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/auto.html\" target=\"_blank\" rel=\"noopener noreferrer\">Automotive Die Casting Parts<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/aircraft.html\" target=\"_blank\" rel=\"noopener noreferrer\">Airplane Die Casting Parts<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/lighting.html\" target=\"_blank\" rel=\"noopener noreferrer\">Light Fixture Die Casting Parts<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/kdcgallery\/index.php\" target=\"_blank\" rel=\"noopener noreferrer\">Consumer Products Aluminum Parts<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/aerospace.html\" target=\"_blank\" rel=\"noopener noreferrer\">Aerospace Die Casting Parts<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/military_parts.html\" target=\"_blank\" rel=\"noopener noreferrer\">Military Die Casting Parts<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/tooling.html\" target=\"_blank\" rel=\"noopener noreferrer\">Die Casting Tooling<\/a><br \/>\n<a href=\"http:\/\/www.cast-parts.com\/diecasting_prices.html\" target=\"_blank\" title=\"Cast Parts Diecasting Prices\" rel=\"noopener noreferrer\">Cast Parts Diecasting Prices<\/a><\/p>\n<p>Die Casting Process<br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/what-is-die-casting.html\" target=\"_blank\" title=\"What is Die Casting?\" rel=\"noopener noreferrer\">What is Die Casting?<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/sandcasting.html\" target=\"_blank\" title=\"Aluminum Die Casting Prices\" rel=\"noopener noreferrer\">Aluminum Die Casting Prices<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/why-use-diecasting.html\" target=\"_blank\" title=\"Why Should You Use Die Castings?\" rel=\"noopener noreferrer\">Why Should You Use Die Castings?<\/a><br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/kinetic_die_casting_company.html\" target=\"_blank\" title=\"Kinetic Die Casting Company\" rel=\"noopener noreferrer\">Kinetic Die Casting Company<\/a><\/p>\n<p><b>Kinetic Die Casting Company<\/b> 6918 Beck Avenue, North Hollywood, California 91605 USA<br \/>\nE-mail <a href=\"mailto:sales@kineticdc.com\">sales@kineticdc.com<\/a> Toll Free: (800) 524-8083 Local: (818) 982-9200 Fax: (818) 982-0877<br \/>\n<a href=\"https:\/\/www.kineticdiecasting.com\/replyform.html\" title target=\"_blank\" rel=\"noopener noreferrer\">Die Casting Parts Prices<\/a><\/p>\n<p>Original Post: <a href='https:\/\/www.kineticdiecasting.com\/kdc\/porosity-in-die-cast-parts-process-2020\/' target='_blank' rel=\"noopener noreferrer\">https:\/\/www.kineticdiecasting.com\/kdc\/porosity-in-die-cast-parts-process-2020\/<\/a><\/p>\n<p><a href=\"http:\/\/www.kineticdiecasting.com\" target=\"_blank\" rel=\"noopener noreferrer\">Kinetic Die Casting Company<\/a> 6918 Beck Avenue North Hollywood California 818-982-9200<\/p>\n<p>No longer interested email from Kinetic Die Casting Blog?. Please email sales@kineticdc.com to unsubscribe<img src='https:\/\/www.kineticdiecasting.com\/kdc\/?es=open&amp;hash=eyJtZXNzYWdlX2lkIjoiMzI2IiwiY2FtcGFpZ25faWQiOiIzIiwiY29udGFjdF9pZCI6IjUyIiwiZW1haWwiOiJhcnRpY2xlMTIzQGNhc3QtcGFydHMuY29tIiwiZ3VpZCI6Inhtc2F1aC11d3pyeGgtenVhZ2N4LXNyZGN1Zi1ha255eGYiLCJhY3Rpb24iOiJvcGVuIn0' width='1' height='1' alt='' \/><\/p>\n","protected":false},"excerpt":{"rendered":"<p>Porosity in Die Cast Parts Process 2020 &#8211; The steel die cavity is sprayed with a liquid release agent to prevent the molten metal from sticking to the steel cavity. Much like the cook will spray a pan before baking a cake. The spray dissipates into steam because the die is very hot. Porosity is [&hellip;]<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[42],"tags":[],"class_list":["post-3822","post","type-post","status-publish","format-standard","hentry","category-cast-parts"],"_links":{"self":[{"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/posts\/3822","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/comments?post=3822"}],"version-history":[{"count":0,"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/posts\/3822\/revisions"}],"wp:attachment":[{"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/media?parent=3822"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/categories?post=3822"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.cast-parts.com\/castings\/wp-json\/wp\/v2\/tags?post=3822"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}